Products

Best results are normally obtained if the firing temperature is as low as possible. select enamels which will fire at 1300-1350 0 f for 20 minutes or more. sifting is not an ideal method of applying the first coat. at these low temperatures individual enamel grains do not flow out easily.
Shijiazhuang zhengzhong technology co.,ltd
Condition:ground coat enamel frits. slide. ... low temperature cobalt-nickel ground glaze/ enamel frit : medium temperature cobalt-nickel ground glaze/ enamel frit : medium temperature nickel ground glaze/ enamel frit : one coat black enamel frit ...
An electroless nickel coating is a dense alloy of nickel and phosphorus. the amount of phosphorus codeposited can range from less than 2% to more than 12%, depending upon bath formulation, operating ph and bath age. the deposition process is auto-catalytic; i.e., once a primary layer of nickel has formed on the substrate, that layer and